PP LGF40 Technical Data
LFT-G® PP LGF40 is a 40% long glass fiber reinforced polypropylene (homopolymer), balancing high stiffness with thin-wall flowability for structural parts that upgrade short-fiber PP and replace heavier ABS, nylon or die-cast metal.
| Property | Specification |
|---|---|
| Product Grade | LFT-G® PP LGF40 |
| Material Type | Long Glass Fiber Reinforced Thermoplastic (LFT) |
| Polymer Matrix | Polypropylene (Homopolymer, HPP) |
| Glass Fiber Content | 40% |
| Available Color | Black / Natural |
| Form | Pellets (Length 10–12mm, customizable 6–25mm) |
Typical Material Properties of PP LGF40
| Property | Value | Standard |
|---|---|---|
| Density | 1.21 g/cm³ | ASTM D-792 |
| Molding Shrinkage | 0.1–0.3% | ASTM D-955 |
| Tensile Strength | 135 MPa | ISO 527 |
| Tensile Modulus | 8,893 MPa | ISO 527 |
| Tensile Elongation | 1.8–2.6% | ISO 527 |
| Flexural Strength | 186 MPa | ASTM D-790 |
| Flexural Modulus | 6,693 MPa | ASTM D-790 |
| Notched Charpy Impact | 35 kJ/m² | ISO 180 |
| HDT (1.8 MPa) | 159 °C | ISO 75-2 |
| Flame Retardant | HB @ 1.5 mm | UL-94 |
Typical values are based on limited laboratory test specimens and are provided for reference only. They are not intended as specification limits. Actual molded-part performance can vary with test conditions, specimen preparation, processing conditions, part design and production batch. Source: official TDS LFT-G® PP-LGF40-NG04-2 (Revised 30/06/2026, version A3).
Mold Compatibility Check: PP LGF40 requires a gate diameter of 5–6 mm. Pin-point gates are not suitable. Please confirm your mold meets this requirement before requesting a trial sample. If your gate is smaller than 5 mm, PP LGF40 cannot be molded in your existing tool - contact us to review alternatives.
PP GF40 vs PP LGF40: Why Engineers Upgrade
PP LGF40 is not a stronger PP GF40. It is a different reinforcement system. In short-fiber PP GF40, the fibres break down to < 3 mm during molding and cannot form a load-bearing skeleton. In PP LGF40, the long fibres survive molding and form a skeleton that carries load, resists creep and absorbs impact. That skeleton is why PP LGF40 holds up under sustained load and sudden impact where short-fiber grades fatigue and crack. The result is a step change in stiffness and long-term performance, not a marginal gain.
It is not a drop-in replacement. PP LGF40 needs a gate diameter of 5–6 mm, and pin-point gates are not suitable (see the check above). When the mold meets this requirement, PP LGF40 can replace PP GF40 in structural parts, and in many cases heavier ABS, nylon or die-cast metal, at lower weight.

Schematic, not to scale: long fibres (10–12 mm) form a load-bearing skeleton, while short fibres (< 3 mm) stay fragmented.
| Property | PP GF40 (Short Fiber) | PP LGF40 (Long Fiber) |
|---|---|---|
| Fiber length in pellet | Short fibres (< 3 mm) | 10–12 mm |
| Fiber skeleton in molded part | Fragmented, no load-bearing skeleton | Load-bearing skeleton |
| Notched impact strength | Lower and inconsistent | 35 kJ/m² (ISO 180) |
| Creep resistance | Lower | Higher |
| Fatigue resistance | Lower | Higher |
| Warpage / shrinkage | Higher, less stable | Lower, more stable |
| Mold requirement | Standard gates | Gate diameter 5–6 mm; no pin-point gates |
PP LGF40 values are from the official TDS (NG04-2). Short-fiber performance varies by grade and supplier. This table compares reinforcement mechanisms, not one competing grade. For a number-to-number comparison, specify the competing grade's TDS.
PP LGF40 Applications
Automotive Electronic Shift Lever Bases
Modern shift-by-wire modules pack intricate, thin-walled structural geometries into tight spaces. PP LGF40 balances the stiffness these parts need with the flowability to fill complex cavities: its 8,893 MPa tensile modulus (ISO 527) holds the lever base rigid under shifting loads, while its 35 kJ/m² Charpy impact (ISO 180) resists cracking under repeated use. At 1.21 g/cm³, it replaces heavier nylon or metal inserts at lower weight.

Industrial Fluid Pump & Valve Housings
Pump and valve housings must hold pressure without creeping or cracking over years of service. PP LGF40's long-fiber skeleton resists creep and sudden fracture, and unlike die-cast brass or steel it does not corrode in water service. Its 6,693 MPa flexural modulus (ASTM D-790) keeps housings rigid under hydrostatic load, while 35 kJ/m² impact strength absorbs pressure surges.

E-Bike & Electric Scooter Chassis Frames
Micro-mobility makers are replacing welded aluminum with single-shot injection molding. PP LGF40 molds footboards and subframes in one shot, cutting assembly steps and weight: replacing a 2.70 g/cm³ aluminum part with 1.21 g/cm³ PP LGF40 gives a theoretical mass reduction of about 55%. Actual outcomes depend on structural redesign and wall-thickness optimization. Its 35 kJ/m² impact strength absorbs urban riding shocks.

How to Mold PP LGF40?
PP LGF40 runs on standard injection molding machines, with two non-negotiable items: a gate diameter of 5–6 mm and pre-drying.

Schematic, not to scale. Numbers refer to the steps below.
① Drying: Dry the pellets for 2–4 hours at 80–90°C, and keep moisture below 0.1%. Long-fiber pellets pick up surface moisture, and wet pellets degrade during molding.
② Melting: Melt at 210–250°C. Use a low-shear screw and avoid overheating, which breaks fibres and degrades the material.
③ Injection: Inject at 69–103 MPa. Keep flow paths open and shear low so the long fibres survive to the part.
④ Gate: Use a gate diameter of 5–6 mm. Pin-point gates are not suitable: they shear the fibres at the gate and destroy the reinforcement. If your gate is smaller than 5 mm, do not run PP LGF40 in that tool.
⑤ Mold: Hold the mold at 38–69°C. Confirm the mold temperature by measurement, not by the machine setting, since mold temperature affects appearance and dimensional stability.
Processing parameters are from the official TDS (NG04-2). Actual settings depend on part design, mold and machine. Validate with a trial sample before production.
Which PP LGF40 Grade Should You Choose?
Start from the job, not the datasheet. The general grade (PP LGF40) is the default answer for structural parts that need stiffness with thin-wall flowability. Move to a special grade only when a specific requirement forces it - outdoor exposure, sustained heat, higher performance, or a tighter budget. Each special grade is a trade-off, not an upgrade on every property. Request the TDS of the grade you choose, and confirm it with a trial sample.
| If you need | Choose | Next step |
|---|---|---|
| General structural parts with no special requirement | HPP LGF40 (General) | Download TDS |
| A lower-cost option for high-volume parts | HPP LGF40-C (Economical) | Download TDS |
| Parts exposed to heat and aging | HPP LGF40 AR (Aging & Heat Retardant) | Download TDS |
| Higher stiffness and strength than the general grade | HPP HLGF40 (High Performance) | Download TDS |
| Outdoor parts exposed to UV | HPP LGF40 V (UV Retardant) | Inquiry to obtain the TDS |
Each variant has its own TDS. Do not apply the general grade's values to a special grade - request the TDS of the grade you choose.
FAQ
Can PP LGF40 replace my current PP GF40 without changing the mold?
In most cases, check the gate first. PP LGF40 needs a 5–6 mm gate; pin-point gates are not suitable. If your mold meets this requirement, the matching 40% content makes it a direct upgrade for stiffness and impact resistance. Send us your gate size and we will confirm.
What gate size does PP LGF40 require?
A minimum gate diameter of 5–6 mm. Pin-point gates shear the long fibres at the gate and destroy the reinforcement, so they are not suitable. If your gate is smaller than 5 mm, do not run PP LGF40 in that tool - contact us to review alternatives.
Can I order a small trial batch before committing to bulk?
Yes. We offer a 25 KG trial MOQ - one bag - so you can validate shrinkage, stiffness and molding behavior on your own machines before scaling up.
Does the general grade resist UV outdoors?
No. The general grade has no UV stabilization. For outdoor parts exposed to sunlight, choose the UV-retardant grade instead - contact us and we will confirm the grade and its TDS.
What does the 159 °C HDT mean for my part?
HDT 159 °C (ISO 75-2) means the material keeps its shape under load up to high temperatures - suitable for parts near heat sources, such as under-hood and appliance components. It is a laboratory value; validate it on your actual part.
What is the difference between HPP and CPP grades?
This page covers HPP (homopolymer), which offers higher stiffness and heat deflection. CPP (copolymer) offers better low-temperature impact resistance. If your part faces cold impact, contact us for the CPP version of this 40% grade.
Request PP LGF40 TDS & Trial Sample
Send us your part drawing and current grade. We will confirm whether PP LGF40 fits, recommend the right variant if needed, and arrange a trial sample.
Ordering grade: LFT-G® PP-LGF40-NG04-2 - 40% LGF, homopolymer (HPP), natural.
Email: Candyhu@lfrtplastic.com
WhatsApp: +86 139 5009 5707

Related Grades
PP LGF40
The optimal 40% balance between stiffness and thin-wall flowability.
Current Grade
PP LGF50
Higher fiber content for parts that need more stiffness than PP LGF40 provides.
Hot Tags: PP LGF40, Long Glass Fiber Polypropylene, Long Fiber Reinforced PP, PP LGF Compound