Question: PPS plus glass fiber is easy to crack, how to improve?
It is a common problem of PPS long glass fiber, stress cracking and post-crystallization shrinkage. The mold temperature is 150 degrees during molding, and the insert is preheated to 200 degrees. It can be solved by adding 180 degrees and more than 2 hours of annealing. Polyphenylene sulfide long glass fiber composite