What Is PA6 LCF50? Key Technical Specifications
LFT-G® PA6 LCF50 (PA6-BC05B) is polyamide 6 melt-impregnated with 50% long carbon fiber, so fiber length, and the load paths it builds, survive the screw and reach the part - where short-fiber grades plateau.
| Product Grade | LFT-G® PA6-BC05B (PA6 LCF50) | Material Type | Long carbon fiber reinforced thermoplastic |
|---|---|---|---|
| Polymer Matrix | Polyamide 6 (nylon 6) | Reinforcement | Long carbon fiber, 50% |
| Standard Color | Black | Available Colors | Black; custom colors on request |
| Pellet Form | Cylindrical long-fiber pellets | Processing Method | Injection molding |
| Property | Value | Standard |
|---|---|---|
| Density | 1.32 g/cm³ | ASTM D-792 |
| Molding Shrinkage | 0.1–0.3 % | ASTM D-955 |
| Tensile Strength | 298 MPa | ISO 527 |
| Tensile Modulus | 34,891 MPa | ISO 527 |
| Tensile Elongation | 0.7–1.5 % | ISO 527 |
| Flexural Strength | 393 MPa | ASTM D-790 |
| Flexural Modulus | 24,058 MPa | ASTM D-790 |
| Notched Izod Impact | 305 J/m | ASTM D-256 |
| Notched Impact Strength | 33 kJ/m² | ISO 179 |
| Notched Impact Strength | 31 kJ/m² | ISO 180 |
| Heat Deflection Temperature | 208 °C | ISO 75-2 |
| Flame Rating | HB at 1.5 mm | UL-94 |
Typical values, PA6-BC05B datasheet Rev. A3; ASTM companion values are in the full TDS.
Inside the part, long fibers interlock into a 3D skeletal network, so parts keep stiffness under vibration, impact and creep.

Learn more about Long Fiber Tech →
How PA6 LCF50 Is Made: Melt Impregnation
These pellets are not extruded from premixed short fibers: carbon fiber rovings are pulled through molten polyamide 6, wetted, then cut to pellet length, so every pellet carries full-length fiber.
Fiber Roving
Continuous carbon fiber bundles feed the line at controlled tension.
Melt Impregnation
Rovings pass through molten PA6, wetting every filament.
Pulling & Cooling
The impregnated strand is pulled and cooled solid.
Pelletizing
Rods are cut into full-fiber-length pellets.

Processing Guidelines & Customization Options
| Parameter | Datasheet Value |
|---|---|
| Pre-Drying | 2–4 hrs at 85–100 °C; dry to below 0.05% moisture |
| Melt Temperature | 243–270 °C |
| Mold Temperature | 54–95 °C |
| Injection Pressure | 69–124 MPa |
| Runner & Gate | Full-round runners, 5–6 mm minimum; large direct gates; no pinpoint gates |
Standard supply is black; custom colors, pellet length and heat or UV stabilization are made to order. In the same family, LCF40 cuts cost and LCF60 maximizes stiffness.
Applications & Metal Replacement Value
LCF50 is picked when aluminum is too heavy and short-fiber nylon too weak.
Automotive Structural Components
Front-end carriers, seat structures and pedal systems move from die-cast aluminum to LCF50 for stiffness per gram; ribs mold in, and 208 °C HDT covers under-hood heat.


Bicycle Wheels & Sports Components
Wheel builders chase stiffness per gram: LCF50 rims hold spoke tension and braking loads at a fraction of metal weight, and shrug off impacts that dent alloy.
Robotic Arms & Automation Links
Robot links pay for every gram twice: in payload and cycle energy. The carbon skeleton holds positional stiffness through millions of cycles on less motor torque.
Drone & UAV Airframes
Airframes buy flight time with grams. LCF50 motor arms hold alignment under thrust and landing loads - corrosion-free, no machining.
Power Tool Housings
Tool shells take drops, vibration and motor heat daily. A rigid LCF50 backbone protects gear trains and screw bosses.
Manufacturing Scale & International Certifications
Produced in Xiamen by a long fiber specialist since 2009; every lot is tested before release and ships with its certificate of analysis.
Quality management systems certified
Material verification and audited provenance
Automotive quality management certified

Frequently Asked Questions
Q1: Can PA6 LCF50 replace die-cast aluminum?
For many brackets, carriers and housings, yes: 298 MPa strength and a 34,891 MPa modulus at 1.32 g/cm³, about half aluminum's density. Send the part and load case for a datasheet check.
Q2: What gate and runner sizes does LCF50 need?
Full-round runners of 5–6 mm minimum and large direct gates, per the datasheet. Pinpoint gates shear the fibers; we review tool designs on request.
Q3: How must LCF50 be dried before molding?
Pre-dry 2–4 hours at 85–100 °C in a dehumidifying dryer, to below 0.05% moisture; wet PA6 splays and loses strength.
Related Grades
The balanced grade: 298 MPa strength at 1.32 g/cm³.
Sample Request & Fast RFQ Channel
Start with verified data: download the full PA6-BC05B datasheet, and send your part and target properties for a sample and molding plan.
WhatsApp Directly: +86 13950095707
Email: candyhu@lfrtplastic.com

Hot Tags: PA6 LCF50, PA6 CF50, long carbon fiber polyamide 6, nylon 6 carbon fiber, PA6-BC05B, LFT-G